环氧砂浆地坪基面要求
添加时间:2020/6/3 16:12:20     浏览次数:
环氧砂浆地坪基面要求
Requirements for base surface of epoxy mortar floor
1,水泥基面牢固、结实、不起壳,应杜绝砂浆起壳现象,混凝土层与砂浆找平层最好一起浇筑。若先浇筑混凝土层,则要求砂浆层的厚度不低于40mm,对叉车道的要求则更厚。有关坡度应符合设计要求,允许偏差值为坡度的2%,并且不大于30mm。
1. The cement base surface shall be firm, firm and free from shell. The phenomenon of mortar shell shall be eliminated. The concrete layer and mortar leveling layer are best poured together. If the concrete layer is poured first, the thickness of the mortar layer is required to be no less than 40 mm, and the requirement for the fork lane is even thicker. The relevant slope shall meet the design requirements, with the allowable deviation of 2% of the slope and no more than 30mm.
2,要求表面不起砂,硬度高,没有水泥粉化现象。新浇筑的水泥砂浆层要充分保养。水泥基面平坦,无凹凸不平、蜂窝麻面、水泥疙瘩,其他涂料、乳胶漆、泡泡糖等残渣。
2. It is required that there is no sand on the surface, high hardness and no cement pulverization. The newly poured cement mortar layer shall be fully maintained. The cement base surface shall be flat and free from unevenness, honeycomb and pockmark, cement pimple, other coating, latex paint, bubble gum and other residues.
3,表面干燥,含水率小于6%,无油污,PH值应在6.0-8.0;水泥地坪养护期过后进场施工前5天,基层不能再用水冲洗或被湿润。
3. The surface is dry, moisture content is less than 6%, no oil stain, pH value should be 6.0-8.0; after the maintenance period of cement floor, 5 days before entering the site for construction, the base course can no longer be washed or wetted with water.
上一页  防腐环氧地坪工艺  
下一页  环氧耐压砂浆地坪养护方法
  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3

Copyright © 技术支持:遨游网络

  • 联系我们
  • 网上订单
  • 工程案例
  • 本站导航

搜索

  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3